Abstract

A novel ceramic synthesis technique, combustion synthesis, was explored to produce red‐emitting Cr3+‐doped Y3A15O12 and Eu3+‐doped Y2O3 phosphors with improved physical and luminescent properties. This technique involves the reaction of metal nitrates (oxidizers) and an organic fuel (urea, carbohydrazide, glycine) at 500°C. Resulting powders are well‐crystallized, with a large surface area and small particle size. The spectral energy distribution was observed using photoluminescence measurements. The effects of processing parameters such as type of fuel, fuelto‐oxidizer ratio, furnace temperature, and batch water content were studied. An increase in phosphor brightness with increasing reaction temperature was observed. Postreaction heat treatments (1000°, 1300°, and 1600°C) increased the luminous intensity of as‐synthesized powders. Residual carbon content and chromium site symmetry were investigated as possible explanations for the increase in brightness with increasing heat treatment temperature. By tailoring the reaction chemistry, the optimal conditions for producing the most luminescent phosphors have been identified.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.