Abstract

Pyrochlore phase free PMN-PT powder of morphotrophic phase boundary (MPB) composition has been prepared using the partial oxalate method. The synthesis process has been optimized by thorough characterization of the intermediate compounds such as columbite and (Mg 1/3Nb 2/3) 0.675 Ti 0.325)O 2 by XRD analysis, particle size analysis, surface area measurement and morphological studies. Lead oxalate produced by in situ precipitation in a suspension of (Mg 1/3Nb 2/3) 0.675Ti 0.325)O 2 powder expected to coat on the particle surface, which improved the homogeneity of the precursors and resulted in the formation of pure PMN-PT phase during calcination at 750 °C. The PMN-PT powder contains more than 95% submicron particle with D 50 0.4 μm. The process eliminates the formation of detrimental pyrochlore phase from the PMN-PT powder.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.