Abstract

Uniform sized and integrated hollow silica spheres with porous shells were prepared by using sulfuric and carboxylic acid-functionalized polystyrene latex spheres as templates, sodium silicate as a precursor, and cetyltrimethylammonium bromide as a shell structure-directing agent. When polystyrene-methyl acrylic acid latex spheres were used as the templates, the pores in the shells of the resultant hollow silica spheres were composed of both micropores and mesopores. The pores in the shells of the hollow silica spheres were mainly composed of mesopores when sulfonated polystyrene-methyl acrylic acid latex spheres were used as the templates. The shell thickness and the specific surface area of the hollow silica spheres increased with the increase in the surface acidity of the latex spheres.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.