Superhydrophobic and crosslinked poly(vinyl alcohol) (PVA)/cellulose nanofibril (CNF) aerogel microspheres were prepared via a combination of the water-in-oil (W/O) emulsification process with the freeze-drying process, followed by thermal chemical vapor deposition of methyltrichlorosilane. The oil phase and the cooling agent were judiciously selected to ensure that the frozen ice microspheres can be easily separated from the emulsion system. The silanized microspheres were highly porous with a bulk density ranging from 4.66 to 16.54mg/cm3. The effects of the solution pH, stirring rate, and emulsifier concentration on the morphology and microstructure of the aerogel microspheres were studied. The highly porous structure of the ultralight aerogel microspheres demonstrated an ultrahigh crude oil absorption capacity (up to 116 times its own weight). This study provides a novel approach for the large-scale preparation of polymeric aerogel microspheres with well-controlled particle sizes that can be used for various applications including oil and chemical spill/leak clean-up.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.