Abstract
Ring-opening polyaddition of 4,4′-disubstituted bisazlactones with various diamines was carried out in N-methyl-2-pyrrolidone to afford polyamides with pendant amide group having inherent viscosities of 0.17-0.51 in quantitative yields. The solution polymerization with aliphatic diamines was almost complete at room temperature within 24 hr. Nearly all of the polyamides were soluble in polar in polar aprotic solvents and in acidic solvents. These polymers began to decompose at around 200–300°C as determined by DTA and TGA under nitrogen.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Polymer Science: Polymer Chemistry Edition
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.