Abstract

The development of efficient method to prepare poly(silyl ether)s (PSEs) is highly desirable. Herein, an environmentally sustainable copper-catalyzed dehydrocoupling polymerization was developed with good yields and high molecular weight (up to 48,400 of Mn and up to 97% yield). Monomers of different types (AB type or AA and BB type) are suitable to afford PSEs. The PSEs show good thermal stability and low glass-transition temperature.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.