Abstract

Nanostructured MgO powders have been synthesized using chemical methods. Ammonium oxalate and Magnesium sulphate were used as the precursor materials. The weight ratios of the raw materials (ammonium oxalate/Magnesium sulphate) were 0.9, 1, 1.1, 1.2, 1.3, and 1.4. As a result of chemical reaction (between them), Magnesium oxalate was synthesized. Produced samples were analyzed by XRD and SEM. The results show that the best ratio (for ammonium oxalate/Magnesium sulphate) is 1.4. Produced Magnesium oxalate powder was heated at 450 and 550°C. The final product was MgO nanopowder. XRD studies indicate that the highest ratio of MgO was observed in the specimen heated at 450°C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.