ABSTRACTNovel polystyrene microsphere (PSMS)-based PSMS/Si and polystyrene/silica nanoparticle/multi-walled carbon nanotube (PS/Si/MWCNT) nanocomposite has been prepared using in situ sol-gel and chemical amalgamation methods. Aniline monomer was introduced by in situ route to form PSMS/PANI, PSMS/PANI/Si and PSMS/PANI/Si/MWCNT nanocomposite. FESEM of nanocomposite indicated core-shell spherical and tubular morphology. Glass transition temperature (Tg) and maximum decomposition temperature (Tmax) of PSMS/PANI/Si/MWCNT nanocomposite were found as 295°C and 524°C, respectively, which were higher than the PSMS/PANI (Tg = 245°C; Tmax = 387°C) and PSMS/PANI/Si (Tg = 257°C; Tmax = 388°C) nanocomposite. For nanocomposite dispersion, tetrahydrofuran was studied as fine solvent. XRD depicted amorphous nature of PSMS/Si and PSMS/PANI/Si; however MWCNT reduced amorphous character of PSMS/PANI/Si/MWCNT. Electromagnetic interference (EMI) shielding effectiveness improved from 0.1 dB (PSMS) to 12.3 dB (PSMS/PANI/Si) to 24.5 dB (PSMS/PANI/Si/MWCNT). The increase in EMI shielding effectiveness was also observed with variation in log of conductivity from −14 mho m−1 (PSMA) to 1.17 mho m−1 (PSMS/PANI/Si/MWCNT).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.