Abstract

Flame‐retarded polyamide 6.6 (FR‐PA6.6) was prepared by the cocondensation of hexamethylene diammonium adipate (AH‐salt) with the corresponding salts of hexamethylene diamine and two different organophosphorus compounds, namely, 3‐hydroxyphenylphosphinylpropanoic acid (3‐HPP, 1) and 9,10‐dihydro‐10‐[2,3‐di (hydroxycarbonylpropyl]‐10‐phosphaphenanthrene‐10‐oxide (DDP, 2). The incorporation of the phosphorus comonomers and the thermal and physical properties of the resulting copolyamides have been studied. The phosphorus‐modified FR‐PA6.6 possesses high relative viscosities of 2.0 to 2.4, good thermal stability, and was used for the production of polyamide blends by merging FR‐PA6.6 with commercial PA6. This offered access to flame‐retarded PA6 multifilaments, which possess tensile strengths up to 0.7 GPa and elastic moduli up to 6.2 GPa. Knitted fabrics of FR‐PA6 exhibit high limiting oxygen index (LOI) values between 36 and 38 and executed burning tests demonstrate that the incorporation of phosphorus‐based comonomers improve flame retardancy significantly. The approach presented here offers a straightforward access to effective flame retardancy in nylon 6.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.