Abstract

Hollow spherical WO3 powder was prepared from mixed solution of ammonium metatungstate, glycine and ammonium nitrate by spray solution combustion synthesis (SSCS) method. The effects of fuel ratio, temperature, precursor solution concentration on the structure and morphology of as-prepared powder, and the SSCS mechanism have been discussed in detail. When precursor solution concentration is 0.10 mol/L, in which the fuel ratio is 2, and reaction temperature set to be 800 °C, the spherical WO3 powder with smooth surface and a median diameter of 24.02 μm can be obtained, which consists of particles with a diameter of about 30 nm, and the specific surface area is 13.5 m2/g. Moreover, the as-synthesized WO3 powder is applied to degrade RhB solution in visible light to evaluate its catalytic performance by PLS-SXE300/300UV. Only 10 mg powder can degrade 70.1% RhB solution within 2 h.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.