A simple strategy involving desilication and recrystallization of silicalite-1 in tetrapropylammonium hydroxide (TPAOH) solution was successfully developed to prepare hollow zeolite nanocubes and three-dimensionally macroporous zeolite monoliths. Large voids were introduced to silicalite-1 crystals by controlled silicon leaching with OH– and thin intact shells were formed by the recrystallization of silicon with TPA+. The size of nanocubes could be easily controlled from ∼150 nm to ∼600 nm by simply adjusting the size of parent silicalite-1. Apart from template function to increase the yield of hollow silicalite-1, TPA+ adsorbed on the zeolite protects the parent crystal surface where the recrystallization occurred. The size of the mesopores and/or macropores in the hollow zeolite shell can be controlled by varying the amount of competitive Na+ adsorbent added to the TPAOH solution. Furthermore, three-dimensional macroporous zeolite monoliths can be formed when an electrolyte, such as NaCl, was added to t...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.