Abstract

Polylactic acid was synthesized from commercial available cheap aqueous lactic acid (85%–90% w/w) using succinic anhydride and SnCl2.2H2O as catalyst in the absence of organic solvents. As a result, polylactic acid with a molecular weight of 60000 was prepared in 10 h. The new procedure is much simple, cheap and outstanding in that the start material is aqueous lactic acid; the catalytic system is environmentally benign.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.