Abstract

A pigment of Fe4N particles for magnetic recording was prepared by nitrogenizing acicular metal iron powder. The chemical treatment needed to obtain stoichiometric Fe4N powder was studied, and it was found that Fe4N powder was obtained when the Fe powder was heated at about 400°C in a mixture of H2–NH3 (65–80 vol.%). The Curie point of the powder coincided well with that of bulk Fe4N. The coercive force of Fe4N was 640 Oe, which is considerably smaller than that of the Fe powder used as the starting material. The dispersion of magnetic anisotropy was measured by a torque meter, and the decrease in the coercivity of nitrogenized iron powder was attributed to the exchange anisotropy of the surface layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.