Abstract

The synthesis and mesomorphic properties of a series of ferroelectric liquid crystalline polysiloxanes bearing chiral 4-[(4-((n-alkyloxy)sulfinyl)phenyl)ethynyl]phenyl 4-(undecyloxy)benzoate as mesogenic pendant groups are presented. In these polymers, the chirality is introduced via an asymmetric sulfur atom. The synthesis of the materials was possible through three successive polymer-analogous reactions. The last key synthetic step is the polyesterification of the poly((undecyloxy)benzoic acid-methylsiloxane) with the n-alkyl 4-[(4-hydroxyphenyl)ethynyl]benzenesulfinate derivatives, which could be carried out efficiently. Up to 97% overall substitution rates of the siloxane units by the mesogenic moiety could thus be obtained. In this paper are also reported the results of the preliminary investigations of the ferroelectric properties, carried out in the S c * phase of one polymer. Finally, the comparison of the mesomorphic properties of a sulfinate-based polymer and molecule with their carboxylate-based counterparts is briefly reviewed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.