Hydrated amorphous FePO 4 was synthesized by a sonochemical reaction method, in which a solution of (NH 4) 2HPO 4 and FeSO 4·7H 2O was irradiated by an ultrasonic wave. From this material, two kinds of cathode materials were easily prepared: (1) an amorphous sample prepared by heating at 350 °C and (2) a crystalline sample prepared by heating at 700 °C. Both samples consisted of homogeneous sub-micron particles. The amorphous sample of FePO 4 exhibited high discharge capacities with more than 100 mAh g −1 in the range of 3.9–2.0 V versus Li/Li + at a current rate of 0.2 C. The sonochemical synthesis proposed herein has the following advantages: no use of oxidation agents for production of trivalent iron ions, reduction in reaction time, control of particle size, and enlargement in surface area for the preparation of the cathode material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.