Sr3B2SiO8 host material doped with separately Eu3+, Dy3+ synthesized by conventional solid state synthesis methods at 1100°C. According to the results of XRD, samples have both of the Sr3B2SiO8 phase and the SrSiO3 phase (Multi-phase MP). Although there is significant amount of impurity concentration, expected energy transitions were obtained from the samples which are doped with Eu3+ and Dy3+. Both samples were performed to the radioluminescence (RL) and photoluminescence (PL) measurements. Measurement results, they were both in harmony with each other. Eu: Sr3B2SiO8 (MP) phosphor has 5D0→7Fj (j=0, 1, 2, 3 and 4) transitions and Dy: Sr3B2SiO8 (MP) phosphor has 4F9/2→6HJ (j=9/2, 11/2, 13/2 and 15/2) transitions. Dy:Sr3B2SiO8 (MP) phosphor synthesized by conventional solid state synthesis method and the RL and PL properties were examined for the first time.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.