Abstract
AbstractWe have prepared two new CaII amidinates, which comprise a new class of ALD precursors. The syntheses proceed by a direct reaction between Ca metal and the amidine ligands in the presence of ammonia. Bis(N,N′‐diisopropylformamidinato)calcium(II) (1) and bis(N,N′‐diisopropylacetamidinato)calcium(II) (2) adopt dimeric structures in solution and in the solid state. X‐ray crystallography revealed asymmetry in one of the bridging ligands to afford the structure [(η2‐L)Ca(μ‐η2:η2‐L)(μ‐η2:η1‐L)Ca(η2‐L)]. These amidinate complexes showed unprecedentedly high volatility as compared to the widely employed and commercially available CaII precursor, [Ca3(tmhd)6]. In CaS ALD with 1 and H2S, the ALD window was approximately two times wider and lower in temperature by about 150 °C than previously reported with [Ca3(tmhd)6] and H2S. Complexes 1 and 2, with their excellent volatility and thermal stability (up to at least 350 °C), are the first homoleptic CaII amidinates suitable for use as ALD precursors.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.