Abstract

We report the fabrication of monolithic bulk amorphous Ni 59Zr 20Ti 16Si 2Sn 3 alloy and amorphous Ni 59Zr 20Ti 16Si 2Sn 3 alloy reinforced Cu matrix composite using a combination of RCRF (Repeated Cold Rolling and Folding) and warm rolling processes. Based on the TTT curve established for the amorphous Ni 59Zr 20Ti 16Si 2Sn 3 alloy, the crystallization of the amorphous ribbon is prevented during warm rolling process. The micro-hardness of the amorphous alloy (600±30 Hv) is comparable with those for other Ni-based amorphous alloys.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.