Abstract

Samples of barite mineral ore, were ground to a mesh of 250, and then were subjected to a leaching stage with hydrochloric acid at different times, then; the leached barite mineral ore was subjected to a carbonation stage controlling different parameters such as pH, temperature, time and speed of agitation. Finally, it was subjected to a sintering stage with the Fe2O3 precursor obtained from the waste powder of the steelmaking company’s rolling process, in a temperature range of 1000 and 1200 ° C, for 12 and 24 times. The materials obtained are characterized by infrared spectroscopy (IR Spectroscopy), X-ray Diffraction (XRD) and Scanning Electron Microscopy (SEM).

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.