Abstract
Eu-doped aluminum nitride phosphors were successfully prepared using simple direct nitridation of a metallic aluminum and Eu2 O3 powder mixture in flowing ammonia. AlN formed at reaction temperatures >900°C, and Eu3+ transformed into the secondary oxide phase EuAl2 O4 in the nitridation condition. Phase pure AlN was obtained by post-heat treatment of the nitridated product at 1600°C for 3h in a nitrogen atmosphere, with an Eu2+ doping concentration<0.5%. The phosphors exhibited broad green emission centered at 521nm under 363nm excitation. The luminescence of the phosphor was significantly influenced by the post-heat treatment temperature, which affected the dissolution of Eu2+ , phase purity, crystallinity, and particle size of the AlN host.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Luminescence : the journal of biological and chemical luminescence
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.