An investigation of the size distribution and phase composition as well an analysis of the Al–Mg–B powder system are performed as a function of the time of mechanical activation in a planetary mill and heat treatment regimes. It is found out that the largest content of the AlMgB14 phase is observed in the materials manufactured from a powder mixture subjected to a 4-hour mechanical treatment and sintered at the temperature 1130°С.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.