Abstract

The effect of ultrasonic treatment (UT) on the synthesis of Al–MgAl2O4 master alloy has been studied by the reaction of SiO2 precursor with Al-2wt% Mg. The results show that SiO2 reaction is enhanced after UT and the corresponding mechanism is proposed. Grain refinement studies in pure Al showed that an increase in addition level of MgAl2O4 particles resulted in two to threefold reduction in grain size; whereas, UT intensified the grain size reduction by 11–12 fold. Significant grain refinement on UT is attributed to the cavitation enhanced wetting which activates MgAl2O4 particles as potent nucleating site for Al.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.