Abstract

A series of CaZrO3:Bi3+, CaZrO3:Eu3+, CaZrO3:Eu3+, Bi3+, and CaZrO3:Eu3+, Bi3+, Li+ phosphors are synthesized by high-temperature solid-state reaction method in air. Their luminescence properties are researched, compared, and analyzed. CaZrO3:Bi3+ phosphor under excitation at 310 nm emits deep-blue light with chromaticity coordinate (0.1612, 0.0254). CaZrO3:Eu3+ phosphor under excitation at 310 and 395 nm shows red-emitting with chromaticity coordinate (0.6386, 0.3611). CaZrO3:Eu3+, Bi3+ phosphor under excitation at 310 nm exhibits a systematically varied hue from deep-blue to red light by changing Eu3+ ion concentration, and that with excitation at 395 nm only emits red light with chromaticity coordinate (0.6386, 0.3611). The energy transfer process from Bi3+ to Eu3+ ions may be indicated by their spectral properties. The optimal Eu3+ and Bi3+ ions concentrations are 5 mol% and 0.9 mol%, respectively. The emission intensity CaZrO3:Eu3+, Bi3+ phosphor may be enhanced about 1.6 times due to the co-doping Li+ ion as charge compensator role. The luminous mechanism of CaZrO3:Eu3+, Bi3+ phosphor is explained by the simplified energy level diagrams of Bi3+ and Eu3+ ions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.