ABSTRACTRecently, the research team synthesized some scandium- and titanium-based oxide compounds, in order to analyze their thermoluminescent (TL) response [1-2]. The oxides mixture Sc2TiO5:Eu2Ti2O7:Sc2O3 was synthesized in equilibrium phase by solid state reaction at 1100 °C / 48 h. The structural characterization was performed by XRD and SEM. The TL properties of this oxide mixture were examined after exposing it to gamma radiation from a 60Co source. The glow curve showed two main glow peaks at 151 °C and 260 °C, yet the curve shape looks quite complex, revealing that it is composed by overlapped individual TL peaks, which was confirmed with the Tstop preheat method performed [3]. The linear dose-response between 150 to 600 Gy was obtained, followed by a slow saturation stage. The intensity of the glow curves increases as the radiation dose increases, and their maxima remain at the same temperature values, which indicates that the TL phenomenon follows first-order kinetics [4]. After ten irradiation-TL readout cycles at 500 Gy, good stability (SD 2.02 %) between TL integrated response and the exposure dose was found. It is concluded that Sc2TiO5:Eu2Ti2O7:Sc2O3 is a promising material to use as high-dose dosimeter.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.