Abstract

Cubical ZrO2 phosphor doped with the europium synthesized by conventional solid state synthesis method. The prepared phosphor was characterized by X-ray diffraction (XRD) technique, field emission gun scanning electron microscopy (FEGSEM) and transmission electron microscopy (TEM). In this paper, we focused on the thermoluminescence glow curves and kinetic parameters, activation energy, order of kinetics, and the frequency factor of ZrO2:Eu3+ phosphor under different doses of UV irradiations at a heating rate of 6.7 °C/s. The kinetic parameters activation energy E, the order of kinetics b, and the frequency factor s of synthesized phosphor of ZrO2:Eu3+ have been calculated by using a peak shape method.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.