Abstract

Gas atomized 4J36 alloy powder was milled for 72 h then mixed with ZrW2O8 powder and sintered at 600°C for 4 h under argon atmosphere. 4J36/ZrW2O8 composites containing 10 vol.%, 20 vol.%, 30 vol.%, and 40 vol.% ZrW2O8 were fabricated, the relative density of which ranged from 70% to 80%. Thermal expansion coefficients of the composites decreased as the amount of ZrW2O8 increased, in agreement with the rule of the mixture. The coefficient of thermal expansion of the 4J36/40 vol.%ZrW2O8 composite in 25–100°C is 0.55 × 10−6/°C.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.