Abstract

AbstractCrosslinked poly(2‐(N,N‐dimethylamino)ethyl methacrylate‐co‐N‐hydroxymethyl acrylamide) poly(DMAEMA‐co‐NHMAAM) copolymers were synthesized using ammonium persulfate (APS)/N,N,N′,N′‐tetramethyl ethylenediamine (TEMED) as initiator/accelerator system in the presence of tetraethyleneglycol diacrylate (TEGDA) as crosslinker in water at 60°C. The effects of comonomer composition in the feed, pH of the swelling medium, and the temperature on the equilibrium swelling (ES) values of hydrogels were investigated. While the initial total monomer concentration was kept constant at 0.5 or 1 mol/l, the contents of APS and TEGDA in the feed were 1 mol% of the total monomers. ES values of DMAEMA‐NHMAAM gels increased with the increase in DMAEMA content in the feed. Although DMAEMA‐NHMAAM hydrogels containing up to 30 mol% were transparent in appearance, the presence of 40% DMAEMA in the copolymer worsened its transparency. ES values of the copolymer gels with high DMAEMA contents increased with both temperature and the pH of swelling medium. Copyright © 2006 John Wiley & Sons, Ltd.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.