Pure ZnO and co-doped (Cu, Ag) ZnO nanoparticles (Zn0.90Cu0.05Ag0.05O) are synthesized by chemical co-precipitation method in the presence of capping agent polyethylene glycol 600 (PEG 600) and annealed at 500 °C for 1h. The XRD measurements indicate that the samples show hexagonal structure without any change and the nanocrystalline size decreased from 12 to 5 nm. SEM images are of hexagonal structure of the ZnO and co-doped ZnO samples, and EDAX spectra reveals that the successful doping concentration of Cu and Ag.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.