Abstract

A series of poly(methylisatin biphenylene) were prepared by superacid-catalyzed polyhydroxyalkylation reaction of N-methyl isatin, 2,2′-dihydroxybiphenyl and diphenyl ether. These polymers have some ether linkages on polymer backbone that render softness and make more elastic. And sulfonic acid groups were introduced by sulfonation reaction with potassium-3-bromopropane sulfonic acid. Their sulfonic acid groups with functionalization and the measurement of apposite parameters for proton exchange membranes (PEMs) were described. The membranes showed comparable IEC (1.59–1.98 meq./g), water uptake (32.72–57.30%), proton conductivity (72.1–109.2 mS/cm), and high thermal stability, and also proton conductivity measurement compared with Nafion 211®.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.