Abstract

The sialon-to-ZrB2 ratio during spark-plasma sintering at pressing load 75 MPa and 1200 – 1600°C influenced the phase composition, Si3N4 and Al2O3 contents in sialon, microstructure and grain size of crystalline phases, relative density, open porosity, linear shrinkage, physicomechanical properties, and the linear correlation between the elasticity modulus and compressive strength of mullite–sialon–ZrB2 samples.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.