A series of sulfonated poly(ether ether ketone)s were successfully synthesized via nucleophilic displacement condensation. The membranes are accordingly cast from their DMSO solutions, and fully characterized by determining the ion-exchange capacity, water uptake, dimensional stabilities, proton conductivity and mechanical properties. Among membranes, the block-7c-3 was successfully synthesized by the reaction of Block-6c with chlorosulfonic acid, with the feed ratio of repeated unit to chlorosulfonic acid of 1:8. The experimental results show that the membrane from block-7c-3 has good mechanical, oxidative and dimensional stabilities together with high proton conductivity (5.15 × 10−2 Scm−1) at 80 °C under 100 % relative humidity. The membranes also possess excellent thermal and dimensional stabilities, in this respect, they are potential and promising proton conducting membrane material for PEM full cell applications.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.