AbstractTwo series of heterocyclic aromatic polymers were synthesized from 4,4′‐(4,4′‐isopropylidenediphenoxy)bis(phthaltic anhydride) and 2,2′‐bis(3,4‐dicarboxyphenyl)hexafluoropropane dianhydride by two‐step method. The inherent viscosities were in the range of 24–45 cm3/g. The effects of the rigid benzoxazole group in the backbone of copolymer on the thermal, mechanical, and physical properties were investigated. These polymers exhibit good thermal stability. The temperatures of 5% weight loss (T5) of these polymers are in the range of 403–530°C in air and 425–539°C in nitrogen. The chard yields of these polymers are in the range of 15–24% in air and 54–61% in nitrogen. These polymers also have high glass‐transition temperatures and a low coefficient of thermal expansion and good mechanical properties. The poly(benzoxazol imide) has a higher tensile strength and modulus than those of neat polyimide. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call