Abstract
A Red emitting with high efficiency Eu3+ doped Sr3La(AlO)3(BO3)4 and Sm3+ doped Sr3La(AlO)3(BO3)4 phosphors has been synthesized by combustion method, meanwhile, the photoluminescence properties of samples are investigated in detail. Morphology by SEM and chromaticity by CIE was studied. The results show that the excitation extends from 340 nm to 420 nm, with the highest excitation (394 nm and 406 nm) being in the violet area for Eu3+ and Sm3+ doping, indicating that the phosphor can correlate well with LED chips. Under violet light excitation of 394nm the phosphor Eu3+ doped Sr3La(AlO)3(BO3)4 and of 406 nm the phosphor Sm3+ doped Sr3La(AlO)3(BO3)4 can emit strong red light showing main emission peaks located at 617 nm and 602 nm are observed respectively. The PL properties implies the excellent stability of the phosphor. These results imply that the importance red phosphors Sr3La(AlO)3(BO3)4:Eu3+ and Sr3La(AlO)3(BO3)4:Sm3+ in W-LEDs under NUV excitation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.