The graphite intercalation compound with large exfoliated volume was prepared by chemical oxidation method. The experimental parameters on the exfoliated volume were discussed in detail. It was found that the optimum preparing conditions went as follows: the mass ratio of graphite flakes:C2H5COOH:FeCl3:CrO3=1:2.8:0.3:0.2, the reaction temperature and time were 30 °C and 40 minutes, respectively. The exfoliated volume of GIC reached up to 575 mL·g1 in the conditions. The composition, structure and properties of the graphite intercalation compound were characterized and analyzed by SEM, TG, DSC, VSM techniques. The millimeter wave (MMW) attenuation performances of GIC were investigated by MMW radar measurement device. The results showed that the MMW attenuation properties of FeCl3-GIC are batter than H2SO4-GIC because of its magnetic absorption for millimeter wave.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.