Abstract

Hydrated lanthanum fluoride powders, both undoped, and doped with erbium and ytterbium fluorides (to a total content of 6–28 mol %), of the general formula RF3 · nH2O (n = 0.30 ± 0.01), crystallizing in the hexagonal system, were obtained by coprecipitation from aqueous solutions of the corresponding nitrates by the interaction with hydrofluoric acid. The dehydration is completed at 380°C. At 600°C, the concentrated solid solution decomposes to precipitate a phase with the structure of orthorhombic YF3. The efficiency of the upconversion luminescence of the powders, excited at a wavelength of 974 nm, is low.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call