Abstract

Pure semi-ionic F-doped graphene with the s-F concentration high up to 17.4 at.% (s-FG-17.4) and covalent F-doped graphene with the c-F concentration of 17.8 at.% (c-FG-17.8) were synthesized by fluorination of graphene respectively at the low temperature of 100 °C and the conventional temperature of 200 °C. The electronic and magnetic properties of the two samples were studied. The results show that s-FG-17.4 is metal and exhibits strong ferromagnetism with the Curie temperature of 229 K and high magnetization of 1.1 emu/g; by contrast, c-FG-17.8 is semiconductor and exhibits spin-half paramagnetism with low magnetization of 0.1 emu/g. Thus, this study provided a reliable method to synthesize high-concentration pure s-FG and proposed an effective sp3 dopants for obtaining metallic and ferromagnetic graphene with high magnetization.