Abstract

Arylenedioxy-organosilanylene polymers with adamantane units in the backbone were prepared by Rh-catalyzed dehydrocoupling of bis(4-hydroxyphenyl)adamantanes with organohydrosilanes, and their heat resistance was evaluated by thermogravimetric analysis in nitrogen. Among these polymers, the highest Td10 (10% weight loss temperature) of 547 °C was achieved for polymer 2a prepared from 1,3-bis(4-hydroxyphenyl)adamantane and phenylsilane. Polymer 2a exhibited good heat resistance even in air with Td10 = 387 °C, and standing of the polymer at 150 °C for 8 h resulted in no evident weight loss

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.