Abstract

Micro-emulsion method is adopted to synthesis rGO-Fe3O4-PANI (reduced graphene oxide-Fe3O4-polyaniline) ternary nano-composites. With the different contents of aniline (0.1 g, 0.2 g, 0.3 g) added in production, the corresponding final products are named as sample 1, sample 2, sample 3, respectively. The results of TEM indicate that the mean size of Fe3O4 nano-particles is 14 nm and they are anchored onto rGO slice. There are some PANI polymer wrinkles distributed on the rGO surface uniformly. The electro-magnetic data demonstrate that sample 1 possess a great enhancement of the electro-magnetic wave absorption abilities and frequency bandwidth among the three samples. The RLmin (minimum reflection loss) value of sample 1 is -44.16 dB at 4.29 GHz with 5 mm coating thickness and 1.77 GHz (3.72-4.94 GHz, 13.33-13.88 GHz) frequency bandwidth (RL <italic/> -10 dB). We can believe that this kind of nano-composites will have a promising application in the future.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call