Abstract

La-doped SrTiO3 (LST) powders were synthesized by ultrasonic spray pyrolysis using an aqueous solution of a metal nitrate. SEM images showed that the as-prepared LST powders had a spherical morphology with a diameter of 1 μm. XRD patterns showed that the crystal phase of the as-prepared powders was amorphous and that the powders crystallized to the perovskite phase by calcination at 900 °C. The sintered LST body had the highest electrical conductivity at a La doping concentration (Lax) of 0.1 under a reducing atmosphere. A solid oxide fuel cell (SOFC) with La0.1Sr0.9TiO3Sm-doped CeO2 (1:9) as the anode exhibited a maximum power density of 137.8 mW/cm2 and an open circuit voltage of 1.08 V at 880 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.