Abstract

Ilmenite is a natural material in the form of sand which contains heavy metal minerals that are very abundant in Lampung province. This research aims to determine the content of TiO 2 from Lampungs iron sand by leaching method with temperature variation. The iron sand are mixed with sodium hydrogen carbonate (NaHCO 3 ), then heated at 700 ◦ C for an hour. This research uses 5 samples with leaching temperature variation of 70, 80, 90, 100, and 110 ◦ C for 2 hours. The acid leaching process uses HCl 12 M with a ratio of iron sand and HCl of 1:4, while the water leaching process uses 50 ml of distilled water. Furthermore, the samples are characterized using XRD and XRF to determine TiO 2 content in the iron sand. The result shows that the highest amount of TiO 2 is obtained in the sample with the leaching temperature of 110 ◦ C for 2 hours, which is approximately 61%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.