Abstract

Copolymer thin films of isoprene with acrylic acid were synthesized using PECVD. In that way, the stretchable functionality of polyisoprene (PI) was combined with the hydrophilic functionality of poly(acrylic acid) (PAA) to obtain stretchable thin films with adjustable wettabilities. Deposition rates were found to change between 9 and 5.5 nm/min depending on the monomer flowrates. The analysis of water contact angle (WCA) values indicated that films having more AA units in their structures were more wettable. The stretchability of the films was assessed on laboratory gloves through stretch-release test and on PET sheet through bend-release test. No significant changes in the WCA values with no observable cracks and failures after successive tests were indication of stretchability of the copolymer films.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.