Silver colloids were produced by chemical reduction of silver salt (silver nitrate, AgNO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> ) solution. As a reducing agents trisodium citrate, sodium borohydride, ascorbic acid, PVP (Polyvinylpyrrolidone) and glucose were used. The characters of silver nanoparticles were investigated using UV-Vis spectrophotometer, dynamic light scattering (DLS), zeta (ζ) potential measurements and scanning electron microscopy. The as prepared silver nanoparticles were used in SERS measurements of pyridine. The best enhancement of the signal was achieved using sample reduced and stabilized with citrate, with the particle size of approximately 40 nm and non-uniform distribution. As aggregating agents NaNO <sub xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">3</sub> , KCl and KBr in different concentrations were tested. The Raman signal for pyridine was enhanced even more with the addition of sodium borohydride instead of other aggregating agents. Addition of borohydride had the largest impact to sample stabilized with DEAE-dextran which consists of large (0.5 μm) as well as very small silver nanoparticles. The mixture colloid-borohydride-pyridine was stable for hours.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.