AbstractThree phthalonitrile monomers containing pyrimidine ring and benzene ring side group were successfully synthesized with 4, 6‐dichloro‐2‐phenylpyrimidine, three kinds of phenols (resorcinol, bisphenol A and bisphenol AF) and 4‐nitrophthalonitrile via nucleophilic substitution reaction. All the phthalonitrile monomers exhibited excellent processing performance due to low melting points (Tm) (below 100 °C) and wide processing windows (difference between melting temperature and curing temperature) above 140 °C. By introducing pyrimidine ring and benzene ring side group, the lower melting point of monomers did not affect the thermal stability and thermal mechanical properties of the phthalonitrile resins based on different bisphenols. In particular, 5 % thermal decomposition temperature (T5%) and glass transition temperature (Tg) of phthalonitrile resin based on resorcinol surpassed 455 and 400 °C while storage modulus (E′) was 3209 MPa. Therefore, phthalonitrile resin containing pyrimidine ring and benzene ring side group have potential applications in the field of high temperature resistant polymers and composites.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call