Abstract

Hexamethylene diisocyanate (HMDI) based polyurethane-urea-amide (PUUA) is synthesized using diamide chain extenders and dihydroxy polystyrene. The rigid segment structure is HMDI-6X6-HMDI. The repeating molecular weight of the soft segment is varied from 2678 to 9202 g mol−1 using HMDI as a chain extender. The inherent viscosity of the polymer is 1.3–3.9 dL g−1. Tm of PUUA varies between 239 and 265 °C. The crystallinity of the amide segments is up to 70%. The polymers show single-stage decomposition temperature around 415 °C. WAXS data confirm the semi-crystalline nature of the polymer. The solvent resistivity of the polymer in chloroform is high due to high crystallinity of the hard segment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.