Abstract
1HNMR, and elemental analysis. The prepared polyester showed inherent viscosity of 0.29 dl/g in NMP at 25 °C, indicating their moderate molecular weight. The Polyester was completely soluble in aprotic polar solvents such as N-methylpyrolidone (NMP), dimethylformamide (DMF), Dimethyl Acetamid (DMAC), dimthylsulfoxide (DMSO). TGA determined the 10% weight loss temperature (T 10 ) at 280 °C and residual weight at 600 °C ca. 41% under nitrogen atmosphere.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.