Abstract

Thermo-responsive microgels with core-shell structure were prepared by free radical emulsion polymerization. The core of microgels was consisted of poly (N-isopropyl acrylamide) (PNIPAM), while the shell was consisted of poly (ethylene glycol) methyl ether methacrylate (POEGMA300). In order to compare the transition behavior of the core-shell microgels with the microgels consisted of one thermo-responsive microgel, PNIPAM and POEGMA300 microgels were prepared. PNIPAM exhibits a lower critical solution temperature (LCST) of 32 °C, and the LCST of POEGMA300 is approximately 63 °C. The thermo-responsive microgel behavior was measured by dynamic light scattering (DLS). It is observed that both of PNIPAM and POEGMA300 microgels show a thermo-responsive ability. The particle size significantly drops when the temperature passes LCST. Moreover the particle size of the thermo-responsive microgels with core (PNIPAM)-shell (POEGMA300) structure shows a linear transition behavior when the temperature is between 50 °C and 70 °C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.