Abstract

Synthesis and characterization of bioglass® of general composition (45-X-Y) SiO2, 24.5 Na2O, 24.5 CaO and 6.0 P2O5 (wt %) was modified by addition of X= (0-1) wt % of CeO2 and Y= (0-1) wt % of La2O3 respectively. These five samples were prepared in alumina crucible via melting route at a temperature of 1400±5 °C with air as a furnace atmosphere. These glass samples were immersed in simulated body fluid (SBF) for different time period and their bioactivity were determined by Fourier transform infrared spectroscopy (FTIR) analysis. Surface morphology was studied by using Scanning electron microscope (SEM). Bioactivity, pH measurement of bioactive glass was carried out and mechanical properties of these glasses increased with increasing concentration of CeO2 and La2O3.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.