Cotton fabric was converted into an ion exchanger by grafting it with (1) glycidyl methacrylate (GMA), followed by aminization with ethylene diamine; (2) dimethylaminoethyl methacrylate (DMAEMA), followed by quaternization; and (3) acrylic acid (AA). Grafting was carried out on a pilot scale using a thiocarbonate–H2O2 redox system. The so-obtained cotton graft copolymers were monitored for their ability to remove different dyes as well as heavy metals from aqueous solutions. It was found that the magnitude of dye exhaustion was as follows. For direct and reactive dyes the percentage of exhaustion follows the order of aminized GMA > quaternarized DMAEMA > DMAEMA, whereas for acid dye the percentage of exhaustion follows the order of quaternarized DMAEMA > DMAEMA > aminized GMA. On the other hand poly(AA)–cotton copolymer is very effective at removal of the basic dye. With respect to heavy metal ions removal, the copolymers show the following order: AA > aminized GMA > quaternarized DMAEMA > DMAEMA. While dichromate removal follows the order of quaternarized DMAEMA > DMAEMA > aminized GMA. © 1998 John Wiley & Sons, Inc. J Appl Polym Sci 68: 2151–2157, 1998

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.