(100-x)ZrO2(x)Bi2O3 (x = 5, 10, 15) system has been synthesized by solid-state reaction technique. Tetragonal Bi7.38Zr0.62O12.31 phase has formed in all the samples after sintering at 850 °C for 24 h. Apart from this, ZrO2 and Bi2O3 are also identified as minority phases. The volume fraction of Bi7.38Zr0.62O12.31 phase increases with increasing concentration of Bi2O3. The AC conductivity plots exhibit phase transition at 570 °C and 460 °C for x = 10 and x = 15 samples, respectively. The maximum conductivity is observed (1.60 mS/cm) in x = 15 sample. These results are correlated and supported with microstructural and thermal analysis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.