It is known that 4CaO⋅Al2O3⋅Fe2O3 (C4AF) mineral gives high sulfate resistance to the cement hardening body in the portland cement. Crystalline C4AF was synthesized at 1300°C from the mixture of CaCO3, Al2O3 and Fe2O3 with a molar ratio of 4:1:1. Glassy C4AF was prepared by quenching the melt with water from 1450°C. Glassy C4AF becomes vitrified by the addition of 7 mass% of SiO2. Mossbauer spectrum showed that the iron in glassy C4AF was distorted. The fraction of the glass in C4AF increase with decreasing hydration speed. Because, C4AF glass formed strongly three-dimensional structure.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.